The Value of Crack Sealing for Asphalt Paved Surfaces
Asphalt paved surfaces are durable, but they can develop cracks due to various factors such as oxidation, traffic load or weather conditions. These cracks, if left unattended can widen, leading to more complex issues. Crack sealing, the process of applying a sealant to cracks in the asphalt, is a crucial maintenance procedure that can increase the lifespan of your asphalt surface and maintain its aesthetic appeal.
The Long-Term Benefits of Crack Sealing
Crack sealing blocks the infiltration of water, one of the most harmful elements for asphalt. When exposed to water, asphalt can erode or develop potholes. Crack sealing effectively seals off the asphalt surface, preventing water from entering and causing damage. Not only does it address the current cracks, but it also helps to prevent new ones from forming, adding years to the lifespan of your asphalt surface.
Regular crack sealing not only protects the integrity of the asphalt but also enhances the aesthetic appeal of your property. Cracked asphalt can give a neglected look to a property. Sealed cracks, on the other hand, give a tidy finish to the property and directly contribute to its visual appeal.
When to Choose Crack Sealing Over Crack Filling
Crack sealing and crack filling solve different problems. Choosing the wrong one wastes money and can shorten the life of the repair. Here is when crack sealing is the right call.
Working Cracks (Cracks That Move with Temperature)
If a crack opens and closes seasonally with temperature changes, it is a working crack. Hot-pour rubberized sealant stays flexible and expands and contracts with the asphalt, so it stays bonded over the long term. Cold-pour filler would crack and pull away within a season or two on a working crack. The Puget Sound's freeze-thaw cycles mean a lot of cracks here are working cracks.
Wider Cracks (Quarter Inch and Up)
Cracks wider than about a quarter inch generally need crack sealing rather than crack filling. The hot-pour material flows deeper into the crack, bonds to the crack walls, and creates a flexible plug that handles the additional movement of a wider crack.
Transverse Cracks Across the Pavement
Transverse cracks (the ones that run perpendicular to traffic) are almost always working cracks because they form from temperature movement. These should be sealed, not filled.
Commercial Parking Lots
On commercial lots, the cost difference between sealing and filling is small relative to the value of avoiding a re-do in two years. We typically recommend crack sealing on commercial work whenever the cracks meet either of the criteria above, even if a few of the cracks would have technically been candidates for filling.
When Crack Filling Is the Better Call Instead
If your cracks are narrow (under a quarter inch), stable (not moving with temperature), and largely longitudinal or surface-level, crack filling is more cost-effective. We will use both methods on the same property when appropriate, sealing the working cracks and filling the stable ones. The right answer often is not one or the other; it is the right method on each crack.
When Both Are Past Their Useful Window
If you have widespread alligator cracking (a network of interconnected cracks resembling alligator skin), neither sealing nor filling will help. The damage is structural. See our alligator cracking guide and asphalt repair page for the right approach.
Our Crack Sealing Process
Crack sealing only works when the prep and application are done right. The actual material is only part of the equation. Here is how we do it on every job:
1. Assessment. We identify all working cracks, measure widths, and confirm which cracks are candidates for sealing versus filling versus patching. Cracks that look similar can need different treatments.
2. Cleaning. Each crack is cleaned out with high-pressure air or hot air to remove debris, vegetation, and old material. A clean crack is what allows the sealant to bond to the crack walls.

3. Heat (when conditions call for it). Hot air lance treatment dries any residual moisture in the crack and warms the crack walls so the hot-pour material bonds tightly.
4. Hot-pour application. Rubberized sealant is heated to roughly 380 to 400 degrees and applied with a pour pot or wand. The material is poured directly into the crack until it fills the void and forms a slight overband at the surface.
5. Cure. Hot-pour sealant cools and sets quickly, typically within 30 to 60 minutes. The treated surface can usually be driven on within a few hours, much faster than sealcoating or paving cure times.

Crack sealing is best performed in dry conditions with surface temperatures above 40 degrees Fahrenheit. In the Puget Sound, that generally means late spring through early fall, though we can sometimes work outside that window when the forecast cooperates.
Minimize Costs with Crack Sealing
Crack sealing is an economically sound practice. It’s far less costly to seal a crack than to deal with major repairs that could arise if water infiltrates to the underlying layers of asphalt. Early maintenance such as regular crack sealing can save substantial costs in the long run and is a worthwhile investment for property owners.
Why Choose Sealcoat Express?
If you need crack sealing in the Puget Sound, here is what working with Sealcoat Express looks like:
- Free assessment with a clear recommendation. We will tell you which cracks need sealing, which need filling, and which need more than either, even if that means recommending less work than you came in expecting.
- Hot-pour rubberized sealant, applied to spec. We use commercial-grade rubberized sealants designed for working cracks in the Puget Sound climate.
- Crews trained on prep, not just application. Most failed crack sealing jobs trace back to cleaning shortcuts. We do not skip steps.
- Same-day return to use. Most crack sealing jobs are drivable within hours of application.
- Straight pricing in writing before any work begins.
Crack sealing is a maintenance investment. Done right and done early, it can add 5 or more years to the life of an asphalt surface. Done late or done wrong, it is wasted money.
Have Questions?
There is a surprising amount to know about all things paving, concrete and beyond. That's why we're here! Don't hesitate to call us at any time!
Crack sealing is a preventative maintenance process where rubberized asphalt sealant is used to seal cracks in an asphalt surface. This procedure prevents water infiltration and fortifies the surface. At Sealcoat Express, we offer professional crack sealing services to prolong the lifespan of your asphalt.
While both procedures aim to address asphalt cracks, crack sealing involves the use of a hot, rubberized sealant, providing a more flexible and durable solution that better withstands thermal expansion and contraction. Crack filling, by contrast, uses cold-pour material and works best on narrower, stable cracks. Sealcoat Express carefully determines the best approach to treat your asphalt surface effectively, and we often use both methods on the same property.
Neglecting to seal cracks can lead to accelerated deterioration of the asphalt, as water and other elements exploit these weak points. Water infiltration is the primary cause of alligator cracking and potholes, both of which require much more expensive asphalt repair than crack sealing would have. Timely crack sealing carried out by a professional company like Sealcoat Express significantly extends the life of your pavement.
While DIY methods exist, a professional service like Sealcoat Express ensures the use of high-quality, commercial-grade materials and appropriate techniques, resulting in a more effective and long-lasting seal.
Generally, crack sealing is best performed in dry conditions and when the temperature is above 40 degrees Fahrenheit. This ensures the sealant adheres to the walls of the crack effectively. In the Puget Sound that typically means late spring through early fall. We also factor in upcoming weather: rain can ruin a fresh application just as it can with sealcoating. At Sealcoat Express, we assess the best conditions to carry out crack sealing for maximum effectiveness.